Nickel Plating Problem

We have six Watts nickel plating tanks, all of which are giving brittle, hard deposits. We have been able to partially solve this problem by diluting the baths 30% by volume. What can we do to solve it on a more permanent basis?

May 1, 2009
Experts Products Finishing

Pitting In NI Sulfamate Tank

We are having problems with pitting in our nickel sulfamate plating bath. What should we do to solve this problem?

Mar 1, 2009
Experts Products Finishing

The Nesting Problem

Our plating shop plates many small parts in barrels. Many of the parts tend to stick together or nest. How can we minimize this problem?

Mar 1, 2009
Experts Products Finishing

Ammeters

I was told that a clamp ammeter is a good thing to have around the plating shop. Where can I purchase one?

Mar 1, 2009
Experts Products Finishing

Nickel and Cooking Surfaces

What do you know about nickel plating regulations on cooking surfaces in Europe? Where can I get a copy of the regulations and tests being done, if any?

Mar 1, 2009
Experts Products Finishing

Distinguishing Acid, Alkaline And Cyanide Zinc Deposits

I need a fast, easy way to determine if a zinc deposit is plated from an acid, alkaline or cyanide plating bath. Do you have any suggestions?

Mar 1, 2009
Experts Products Finishing

Cleaning Before Plating

Our plating operations constantly have problems with surface cleaning prior to plating. Can you offer me any insight on how to solve this problem?

Feb 1, 2009
Experts Products Finishing

Offshoring Issues

Do you have any suggestions or for how we could improve the process of offshoring our production?

Jan 1, 2009
Experts Products Finishing

Flaking Zinc Plate

We have a customer who returned zinc-nickel plated parts to us which we processed in 2005 and have traveled to Asia. The plating is flaking from the parts. Our company is paying for this rework, yet I don’t think we are responsible for redoing the flaking parts. Do you have any thoughts on this?

Jan 1, 2009
Experts Products Finishing

HAZY EMBLEMS

How can I prevent a hazy appearance when I gold plate car emblems and small items found around the home?

Dec 1, 2008
Experts Products Finishing

HEAT TREATED PARTS

Can you suggest a good way of removing oil from parts that have been heat treated followed by quenching?

Dec 1, 2008
Experts Products Finishing

PLATING ON TITANIUM

I am looking for a good procedure for plating copper on commercially pure titanium.